Neodymium Magnets Coating Info
Coating | Thickness | Color | Characteristic |
Nickel | 10-12 um | Bright/Semi-bright | Excellent resistance to humid atmosphere |
Nickel Copper Nickel | 10-12 um | Bright/Semi-bright | Superior resistance to humid atmosphere |
Nickel Copper Semi-bright Nickel | 10-12 um | Bright | Most commonly used coating, price beneficial, excellent against humidity |
Nickel Copper Epoxy | About 25 um | Black | Superior climatic and salt spray resistance |
Nickel Copper Nickel Golden | 12-15 um | Golden | The gold layer is very thin with excellent wear resistance, high hardness, corrosion resistance, and high conductivity. |
Nickel Copper Nickel Stannum | 12-18 um | Silver semi-bright | Superior resistance to humid atmosphere |
Nickel Copper Zinc | About 15 um | Silver semi-bright | Excellent resistance to salt spray |
Nickel Stannum | 12-18 um | Silver semi-bright | Superior resistance to humid atmosphere |
Black Nickel | 10-12 um | Black | Provide corrosion resistance and maintain electrical conductivity while reducing reflectivity on the surface |
Bright Nickel | 10-12 um | Bright | Superior resistance to humid atmosphere |
Epoxy | About 15 um | Black | Superior climatic and salt spray resistance |
Zinc | 4-8 um | Blue white-shining | Good resistance to salt spray |
Dark Zinc | 4-8 um | Black | Offer additional corrosion protection |
Color Zinc | 4-8 um | Color shining | Excellent resistance to salt spray |
Trivalent Zinc | 4-8 um | White-blue | Good resistance to salt spray |
Passivation | About 3 um | Silver grey/black | Offer corrosion protection and improve friction properties of sliding components |